100% Polyester90.000 cyclesPilling resistance 4-5Fastness to rubbing dry 4-5fastness to rubbing wet 4-5Thread displacement 2.7-3.2 mm WARP / 4.6-5.0 mm WEFT
Loading Packaging
No packaging found
Grammage m2 280 g/m² +/-5%
Composition 100% Polyester
Usable width min. 140cm
Martindale Test 90000->100000
Thread displacement 2,7-3,2 mm WARP / 4,6-5,0 mm WEFT
Pilling resistance 4-5
Fastness to rubbing dry 4-5
Fastness to rubbing wet 4-5