Furniture Components
Toptextil
Greta Collection Toptextil
Composition 100% Recycled Poliester
Basis weight 315 g/m²
Width 142 ± 3 cm
Abrasion resistance >100 000 strokes (rubs)
Davis Fabrics
Gusto LN Collection Davis
Grammage m2 240g/m² +/-10%
Composition 100% PES
Usable width min. 140cm
Martindale Test 45000-50000
Thread displacement 3,6-3,9 mm WARP / 3,6-3,9 mm WEFT
Pilling resistance 4-5
Fastness to rubbing dry 5
Fastness to rubbing wet 4
Toptextil
Hamilton Collection Toptextil
Composition 100 % PES
Basis weight 300 g/m² ± 5 %
Width 142 ± 3 cm
Abrasion resistance 30 000 cycles (category B)
Fargotex
Hazel Collection FG
Fabric type| woven fabric
Composition| 100% recycled polyester
Weight| 284 g/m² ± 5%
Width| 140 cm ± 2 cm
Toptextil
Hevia Collection Toptextil
## Composition 100% PES

## Basis weight 440 g/m2 +/- 5%

## Width 142 cm +/- 3 cm

[](https://www.toptextil.pl/en/collections/petproof/)

### [Resistant to snagging](https://www.toptextil.pl/en/collections/petproof/)

[](https://www.toptextil.pl/en/collections/fireretardent/)

### [Cigarette test](https://www.toptextil.pl/en/collections/fireretardent/)

[

### Oeko Tex® Standard 100

](https://www.toptextil.pl/en/collections/oekotex/)

Toptextil
Horton Collection Toptextil
Composition 100% PES
Basis weight 350 g/m2 +/- 5%
Width 142 cm +/- 3 cm
Abrasion resistance 40 000 suwów (rubs)
Davis Fabrics
Hygge Collection Davis
Grammage m2 280 g/m² +/-5%
Composition 100% Polyester
Usable width min. 140cm
Martindale Test 90000->100000
Thread displacement 2,7-3,2 mm WARP / 4,6-5,0 mm WEFT
Pilling resistance 4-5
Fastness to rubbing dry 4-5
Fastness to rubbing wet 4-5
Toptextil
Hygge Collection Toptextil
Composition 100 PES
Basis weight 240 g/m² ± 5 %
Width 142 ± 3 cm
Abrasion resistance 100 000 rubs
Fargotex
Impresso Collection FG
Fabric type| woven fabric
Composition| 60% polyester, 40% acrylic
Weight| 580 g/m² ± 5%
Width| 140 cm ± 2 cm
Martindale abrasion| 75 000 cycles
Fire resistance| BS: 5852: Part 1: 1979, source 0 (cigarette)
Davis Fabrics
Inari Collection Davis
Grammage m2 260 g/m² +/-5%
Composition 100% PP
Usable width min. 140cm
Martindale Test 45000-50000
Thread displacement 3,6-4,0 mm WARP / 3,3-3,7 mm WEFT
Pilling resistance 4
Fastness to rubbing dry 5
Fastness to rubbing wet 5